當雙組份膠在混合過(guò)程中就發(fā)生局部固化時(shí),膠槍打出來(lái)的膠就會(huì )出現結皮或硫化現象。出現這一現象的原因主要有三種:
When the two-component rubber is partially cured in the mixing process, the rubber produced by the rubber gun will be skinned or vulcanized. There are three main reasons for this phenomenon:
⑴膠體顏色較黑,固化快時(shí),可能是由于B組分比例過(guò)高,過(guò)多的催化劑促使固化速度加快。此時(shí),需要適當降低B組分的比例,將結皮或硫化膠沖洗干凈后施工;
⑴ when the colloid color is black and the curing speed is fast, it may be due to the high proportion of component B and too much catalyst to accelerate the curing speed. At this time, it is necessary to properly reduce the proportion of component B and wash the crust or vulcanizate before construction;
⑵若打膠過(guò)程中伴有出膠慢的現象時(shí),可能是混合芯長(cháng)時(shí)間未清洗或清洗不徹底,膠體結皮堵塞管道。因此,定期清洗靜態(tài)混合器是很有必要的。
(2) if the glue is slowly discharged during the gluing process, the mixing core may not be cleaned for a long time or not completely, and the colloidal crust blocks the pipeline. Therefore, it is necessary to clean the static mixer regularly.

⑶當固化和出膠速度均無(wú)異常,而打出的膠仍有結皮或硫化現象時(shí),則可能是設備停機時(shí)間較長(cháng),膠槍未清洗或洗槍不夠徹底,需要將結皮或硫化膠沖洗干凈后后施工。
(3) when there is no abnormality in the curing and rubber outlet speed, and the rubber is still crusted or vulcanized, the equipment may be shut down for a long time, the rubber gun is not cleaned or the gun is not cleaned thoroughly, so it is necessary to wash the crusted or vulcanized rubber before construction.
般而言,膠體本身是沒(méi)有氣泡的,膠體夾有的氣泡極可能是運輸或施工過(guò)程中混入了空氣,如:⑴更換膠桶時(shí)排氣未排干凈;⑵組分在上機后壓盤(pán)未壓下去,導致排泡不徹底。 因此,在使用前排泡要徹底,使用過(guò)程中應正確操作打膠機,保證密封從而阻止空氣進(jìn)入。若懷疑產(chǎn)品自身就帶有氣泡,可以通過(guò)蝴蝶試驗來(lái)進(jìn)行判斷。頭條萊垍
Generally speaking, the colloid itself has no bubbles, and the bubbles contained in the colloid are likely to be mixed with air during transportation or construction, such as: (1) the exhaust is not discharged completely when replacing the rubber barrel; (2) after the components are put on the machine, the pressure plate is not pressed down, resulting in incomplete bubble discharge. Therefore, the foam should be thoroughly before use. During use, the glue applicator should be operated correctly to ensure sealing, so as to prevent air from entering. If it is suspected that the product itself has bubbles, it can be judged by butterfly test. Headline Lai long
- 中空玻璃生產(chǎn)線(xiàn)解決:中空玻璃合片總出錯,返工、漏風(fēng)、粘不牢的難題 2025/12/24
- 合片+充氣+板壓一步到位!中空玻璃生產(chǎn)線(xiàn)效率品質(zhì)雙飆升 2025/12/23
- 玻璃涂布機設備:丁基膠在涂布過(guò)程中產(chǎn)生氣泡的原因分析 2025/12/23
- 中空玻璃生產(chǎn)線(xiàn)的PLC控制系統一鍵操作精準把控生產(chǎn)細節 2025/12/20
- 中空玻璃丁基膠涂布機在打膠中斷膠是怎么回事?如何避免 2025/12/20
- 全自動(dòng)丁基膠涂布機如何解決漏白和內溢? 2025/12/19
- 為啥玻璃廠(chǎng)都搶著(zhù)上大型中空玻璃生產(chǎn)線(xiàn)?4 個(gè)核心原因太戳心! 2025/12/19
- 玻璃廠(chǎng)老板注意!丁基膠涂布機打膠有氣泡?這臺設備徹底解決! 2025/12/19
- 春節停機別忘保養!中空玻璃加工設備這樣維護,開(kāi)春開(kāi)機不趴窩 2025/12/18
- 1分鐘看懂全自動(dòng)中空玻璃生產(chǎn)線(xiàn)!全程不用人工搬太爽了 2025/12/18
產(chǎn)品分類(lèi)Product categories
聯(lián)系我們Contact us
- 咨詢(xún)熱線(xiàn):0531-85717458 13705446998
- 公司地址: 山東省德州市齊河安頭鄉企巢工業(yè)園
- 掃碼聯(lián)系我們:

當前位置: